SAE ARP1631A

Manufacturing Sequence for Fabrication of High-Strength Steel Parts 300M or 4340 Modified Low-Alloy Steels 270,000 psi (1860 MPa) Tensile Strength and Higher

SAE International , 06/24/2024

Publisher: SAE

File Format: PDF

$47.00$94.00


SAE ARP1631A PDF

This document establishes the requirements for sequencing processes relating to parts fabricated from 300M or 4340 modified steel heat treated to, or to be heat treated to 270,000 psi (1860 MPa) minimum ultimate tensile strength (UTS) and higher.