Standard Test Method for Determination of Residual Acrylonitrile Monomer in Styrene-Acrylonitrile Copolymer Resins and Nitrile-Butadiene Rubber by Headspace-Capillary Gas Chromatography (HS-CGC)

ASTM International , 09/01/2016

Publisher: ASTM

File Format: PDF

$37.00$75.00


1.1This test method covers the determination of the residual acrylonitrile (RAN) content in nitrile-butadiene rubbers (NBR), styrene-acrylonitrile (SAN) copolymers, and rubber-modified acrylonitrile-butadiene-styrene (ABS) resins.

1.2Any components that can generate acrylonitrile in the headspace procedure will constitute an interference. The presence of 3-hydroxypropionitrile in latices limits this procedure to dry rubbers and resins.

1.3The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.

1.4This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Specific precautionary statements are given in 6.3 and 6.4.

Note 1:There is no known ISO equivalent to this standard.

ASTM D5508-16 History

ASTM D5508-23

ASTM D5508-23

$31.00 $63.00

ASTM D5508-16

ASTM D5508-16

$37.00 $75.00

ASTM D5508-94a(2009)e1

ASTM D5508-94a(2009)e1

$30.00 $60.00

More ASTM Standards PDF

IEC 62093 Ed. 1.0 b:2005

IEC 62093 Ed. 1.0 b:2005

$129.00 $259.00

IEC 60076-10-1 Ed. 1.0 b:2005
IEC 60851-4 Ed. 2.2 b:2005
IEEE 1050-2004

IEEE 1050-2004

$43.00 $87.00