• SAE AMS5841E

SAE AMS5841E

Cobalt-Nickel Alloy, Corrosion and Heat Resistant, Bars 19Cr 36Co 25Ni 7.0Mo 0.50Cb (Nb) 2.9Ti 0.20Al 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated For Work Strengthening

SAE International , 08/01/2006

Publisher: SAE

File Format: PDF

$30.00$61.00


This specification covers a high strength, corrosion and heat resistant cobalt-chromium-nickel alloy in the form of bars.

These bars have been used typically for applications requiring a combination of high strength up to 1100 degrees F (593 degrees C), good tension-tension fatigue strength, toughness, and ductility, but usage is not limited to such applications. This alloy exhibits exceptionally good resistance to corrosion, crevice-corrosion, stress-corrosion cracking, and elevated temperature relaxation.

SAE AMS5841E History

SAE AMS5841G

SAE AMS5841G

$34.00 $69.00

SAE AMS5841F

SAE AMS5841F

$30.00 $61.00

SAE AMS5841E

SAE AMS5841E

$30.00 $61.00

More SAE Standards PDF

SAE J2931/6_201508

SAE J2931/6_201508

$28.00 $56.00

SAE J2175_201506

SAE J2175_201506

$25.00 $50.00

SAE AMS03_2

SAE AMS03_2

$64.00 $128.00

SAE AS4218

SAE AS4218

$20.00 $41.00