• SAE USCAR5-4

SAE USCAR5-4

AVOIDANCE OF HYDROGEN EMBRITTLEMENT OF STEEL

SAE International , 07/30/2012

Publisher: SAE

File Format: PDF

$25.00$50.00


This standard outlines the conditions that enhance the risk of hydrogen embrittlement of steel and defines the relief procedures required to minimize the risk of hydrogen embrittlement. It is intended to control the process.

Hydrogen embrittlement of steel, which can cause brittle fractures under stress, occurs as a result of the absorption of hydrogen during cleaning, phosphate coating and plating processes. The susceptibility to hydrogen embrittlement increases with increasing stress (internal or externally applied stress) and increasing material strength.

Hardness readings in this specification are in Vickers scale. SAE J417 should be referred to for conversion to other scales.

SAE USCAR5-4 History

SAE USCAR5-5

SAE USCAR5-5

$31.00 $63.00

SAE USCAR5-4

SAE USCAR5-4

$25.00 $50.00

SAE USCAR5-3

SAE USCAR5-3

$25.00 $50.00

More SAE Standards PDF

SAE AS4231D

SAE AS4231D

$28.00 $57.00

SAE AS5459C

SAE AS5459C

$31.00 $63.00

SAE AS6462B

SAE AS6462B

$43.00 $87.00

SAE AMS5607F

SAE AMS5607F

$30.00 $61.00